Description
Performance:
Used for beryllium addition in aluminum alloy smelting, low temperature of addition and low loss of beryllium.
Usage:
1. Bake and dry before use.
2. Add temperature: above 700℃.
3. The added amount of this product: 0.1 ~ 0.5% or determined by the test.
4. Add method: remove scum, put the product into aluminum liquid, stir evenly, and let stand for 5 ~ 10 minutes.

Used for beryllium addition in aluminum alloy smelting, low temperature of addition and low loss of beryllium.
Usage:
1. Bake and dry before use.
2. Add temperature: above 700℃.
3. The added amount of this product: 0.1 ~ 0.5% or determined by the test.
4. Add method: remove scum, put the product into aluminum liquid, stir evenly, and let stand for 5 ~ 10 minutes.

Shape and packing:
Each W.: Around 500g/pc.
Packing: 200 kgs/wooden case.