Description
Performance:
Used for adding silicon element in aluminum alloy smelting, adding temperature is low, composition control is accurate.
Usage:
1. Bake and dry before use.
2. Add temperature: above 700℃.
3. The amount of this product is determined by calculation and test.
4. Adding method: remove scum, put the product into aluminum liquid, melt it, mix it evenly, sample analysis, and pour it after qualified ingredients. In large quantities, it can be melted together with aluminum ingots.
Used for adding silicon element in aluminum alloy smelting, adding temperature is low, composition control is accurate.
Usage:
1. Bake and dry before use.
2. Add temperature: above 700℃.
3. The amount of this product is determined by calculation and test.
4. Adding method: remove scum, put the product into aluminum liquid, melt it, mix it evenly, sample analysis, and pour it after qualified ingredients. In large quantities, it can be melted together with aluminum ingots.
Shape and packing:
Each W.: Around 8 kg.