Description
Performance:
Used for adding iron in aluminum alloy smelting, low temperature and accurate composition control.
Usage:
1. Bake and dry before use.
2. Add temperature: above 720℃.
3. The amount of this product is determined by calculation and test.
4. Adding method: remove scum, put the product into aluminum liquid, melt it and stir it evenly, then stand still for 5 ~ 10 minutes. Or melt with aluminum ingots.
Used for adding iron in aluminum alloy smelting, low temperature and accurate composition control.
Usage:
1. Bake and dry before use.
2. Add temperature: above 720℃.
3. The amount of this product is determined by calculation and test.
4. Adding method: remove scum, put the product into aluminum liquid, melt it and stir it evenly, then stand still for 5 ~ 10 minutes. Or melt with aluminum ingots.
Shape and packing:
Each W.: Around 8 kg.
Packing: 1000 kgs/pallet, wrapped with heat shrinkage film.