Description
Performance:
Used for adding manganese in aluminum alloy smelting. Low temperature and accurate composition control.
Usage:
1. Bake and dry before use.
2. Add temperature: above 700℃.
3. The amount of this product is determined by calculation and test.
4. Add method: remove scum, put the product into aluminum liquid, stir evenly, and let stand for 5 ~ 10 minutes.
Used for adding manganese in aluminum alloy smelting. Low temperature and accurate composition control.
Usage:
1. Bake and dry before use.
2. Add temperature: above 700℃.
3. The amount of this product is determined by calculation and test.
4. Add method: remove scum, put the product into aluminum liquid, stir evenly, and let stand for 5 ~ 10 minutes.
Shape and packing:
Each W.: Around 8 kg.
Packing: 1000 kgs/pallet, wrapped with heat shrinkage film.